Bonding Galvanised Steel: Why It's Difficult and Which Glue to Use

The short answer: galvanised steel is hard to bond because the zinc coating, not the steel, is what the adhesive has to stick to, and some coatings are brittle or carry ingredients that resist bonding. For joints that see movement or impact, Forgeway recommends a flexible MS polymer such as Formoa 017FE. For higher strength where there's little movement, they suggest a structural adhesive such as Purok VX60. Whichever you choose, test on your own galvanised steel first, because results vary from supplier to supplier.

This post is for vehicle builders, trailer makers and fabricators who need to glue galvanised steel and want to know why it sometimes goes wrong. It draws on Forgeway's article Galvanised steel can be a nightmare to bond.

Formoa 017FE white flexible structural adhesive 290ml cartridge

Why is galvanised steel so difficult to bond?

Not all of it is. Forgeway's point is that bondability depends on the grade and the supplier, so one batch can bond perfectly and the next can let go. There are four reasons.

  • The coating process. Hot-dip galvanising forms a metallurgical bond with the steel. Electro-galvanised coatings are thinner. Galvannealed coatings, where iron diffuses into the zinc, are harder and more brittle.
  • Brittle coatings crack under strain. When the joint is loaded, a brittle coating can fail before the adhesive does. A rigid adhesive makes this worse, because it passes all the stress straight into the coating. Hot-dip coatings are somewhat brittle too.
  • Surface chemistry. Zinc itself isn't a low surface energy material, but other ingredients in the coating can leave a surface layer that is. Grease, dirt and other contamination make it worse.
  • Adhesive incompatibility. Some acrylic, epoxy and polyurethane adhesives contain raw materials that don't form a strong chemical bond with zinc.

Which glue should you use on galvanised steel?

Forgeway's guidance is to look for an adhesive with more than 50% elongation, so it can flex without overloading the coating. Hybrid (MS) polymers generally bond well to galvanised steel and are flexible, but they rarely go above 5 MPa, which some companies don't consider structural. So the choice depends on the job:

What the joint needs Forgeway's suggestion Key figures
Movement, vibration or impact Formoa 017FE (MS polymer) About 2.5 MPa on galvanised steel, 300% elongation
Strength, with little movement or impact Purok VX60 Ask us for the data sheet
Very high strength Forgeway structural acrylic 25 MPa shear on electro-galvanised steel, 15% elongation

Note the trade-off in that last row: a lot more strength, but far less give. On a brittle coating, that's exactly where you need to test carefully.

Why is Formoa 017FE a good fit for galvanised steel?

Because most galvanised steel we're asked about is on trailers, vehicle bodies and frames that move. On those, the biggest risk isn't the adhesive being too weak, it's a rigid bond cracking the coating. 017FE stretches up to 300% before it breaks, so it takes the movement instead of handing it to the zinc. It also bonds and seals in one bead, and it's isocyanate- and solvent-free.

The same reasoning is behind our recommendation in our aluminium glue post and our stainless steel post.

Where does 017FE lose on galvanised steel?

  • High-load joints that mustn't move. At around 2.5 MPa on galvanised, it won't do the job of a structural acrylic. Ask us about Purok VX60 or Forgeway's structural acrylics.
  • Dirty steel. MS polymers need a clean, uncontaminated surface. Oily or contaminated galvanising will let it down.
  • Thick to apply. Use a powered applicator for regular work.

How should you prepare galvanised steel?

Forgeway's one firm rule is that the surface must be clean and free from contamination. In practice, that means wiping off grease and dirt with a suitable solvent and letting it dry. Abrasive prep is a judgement call on galvanised steel, because you don't want to cut through a thin coating, so test both ways if you're unsure.

How can you check the bond before you commit?

Forgeway is clear that testing with your exact steel and adhesive is the only real proof. This is the simple test we recommend:

  1. Take an offcut of the galvanised steel you'll be using and mark out three lanes about 100 mm apart.
  2. Leave lane one as received. Clean lanes two and three with isopropyl alcohol on a lint-free cloth.
  3. Once dry, wipe lane three with Formoa Surface Activator, in one direction, and let it flash off.
  4. Run two heavy beads of adhesive down each lane and leave them to cure for at least 7 days.
  5. Try to pull each bead off. If it peels away without a knife, you have an adhesion problem. If you have to cut it off, the bond is good.

The results tell you how much preparation your particular steel needs. If none of the lanes pass, talk to us before you go further.

How much does it cost?

At Gludog, checked November 2026: Formoa 017FE 290 ml is £11.95, the 600 ml foil pack is £15.15 and Surface Activator is £15.49 a litre. Purok VX60 and Forgeway's structural acrylics aren't listed online, so email us for prices.

What should you do next?

Run the three-lane test on your own steel. Then email sales@gludog.com with your results, the coating type if you know it, and what the joint has to do. We'll tell you whether 017FE is enough or whether you need something stronger.

Based on Forgeway's article on bonding galvanised steel. Strength figures are Forgeway's. Prices checked November 2026.